Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 19.3 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 19.3 - 20.3 µm/m-°C

@Temperature 20.0 - 300 °C
10.7 - 11.3 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6
Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo..
CTE, linear 19.3 - 20.3 µm/m-°C

@Temperature 20.0 - 300 °C
10.7 - 11.3 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x
Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all..
CTE, linear 19.3 µm/m-°C

@Temperature 0.000 - 649 °C
10.7 µin/in-°F

@Temperature 32.0 - 1200 °F
Crucible Steel 321 Chromium-Nickel Steel
Crucible 321 is a non-hardenable, low carbon austenitic chromium-nickel steel which is particularly adaptable for parts fabricated by welding without postweld annealing for use at temperatures betwe..
Copyright © lookpolymers.com All Rights Reserved