Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 168 µm/m-°C @Temperature <=100 °C |
93.3 µin/in-°F @Temperature <=212 °F |
ISO E 830 |
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |