Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, 10% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, 30% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, 50% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW, as welded, notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, SMAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, SMAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 0.000 - 316 °C |
9.00 µin/in-°F @Temperature 32.0 - 600 °F |
|
Crucible Steel 316L Chromium-Nickel Steel Crucible 316L is a non-hardenable, low carbon austenitic chromium-nickel steel with superior corrosion and heat resisting qualities. Crucible 316L is designed for special applications requiring resi.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 22.8 °C |
9.00 µin/in-°F @Temperature 73.0 °F |
MD; ASTM D696 |
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
(discontinued **) AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber .. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, SMAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, GMAW, as welded, notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, 904L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW spray weldment, 12.7 mm (1/2 in.) thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, SMAW weldment, 19.1 mm thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 877 °C |
9.00 µin/in-°F @Temperature 68.0 - 1610 °F |
|
Kennametal Stellite Stellite® 25 Cobalt Chromium Cast Alloy Stellite alloy 25 forms a protective oxide film during hot metal-on metal wear which prevents metal transfer and damage due to adhesion. The alloy is resistant to thermal cracking and surface fatig.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, 6.4-19.1 mm thick plate, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, GTAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 24.0 - 982 °C |
9.00 µin/in-°F @Temperature 75.2 - 1800 °F |
|
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 1000 °C |
9.00 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy The higher tungsten content of Stellite alloy 4 gives improved high temperature properties and an increase in abrasive wear resistance over Stellite alloy 6, but not as good as Stellite alloy 12 or .. |