Polymer Property : CTE, linear = 144 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 144 µm/m-°C

@Temperature 200 - 300 °C
80.0 µin/in-°F

@Temperature 392 - 572 °F
ASTM E831
3M Dyneon™ CC191-HE Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company
CTE, linear 144 µm/m-°C

@Temperature <=100 °C
80.0 µin/in-°F

@Temperature <=212 °F
ISO E 830
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy
Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor..
CTE, linear 144 µm/m-°C

@Temperature 150 - 200 °C
80.0 µin/in-°F

@Temperature 302 - 392 °F
Alpha 2
Tra-Con Tra-Bond 526M05 Rapid Low Temperature Cure Adhesive
TRA-BOND 526M05 is a low viscosity, fast cure at low temperature, long pot-life adhesive. Information provided by Tra-Con Inc.
CTE, linear 144 µm/m-°C

@Temperature 100 - 150 °C
80.0 µin/in-°F

@Temperature 212 - 302 °F
ASTM E831-00
DSM Somos® 9420 Epoxy Resin for Stereolithography
DescriptionDSM Somos® 9420 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance and a wid..