Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 235 µm/m-°C @Temperature 20.0 °C |
131 µin/in-°F @Temperature 68.0 °F |
Cured property; alpha 2 |
Aptek 2712-A/B Very low stress silicone adhesive Very low stress silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space gradeAPTEK 2712-A/B is a two component, white, very soft, thixotropic, electrically insulative, silicone ad.. |