Polymer Property : CTE, linear = 13.28 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 13.28 µm/m-°C

@Temperature 21.0 - 538 °C
7.378 µin/in-°F

@Temperature 69.8 - 1000 °F
Latrobe Lescalloy® M50 VIM-VAR High Performance Bearing Steel
LESCALLOY M50 VIM-VAR steel is a through-hardening grade with high hardness and high compressive strength at elevated temperatures. It is produced exclusively as a double vacuum melted produced usi..