Latrobe Lescalloy® M50 VIM-VAR High Performance Bearing Steel

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , High Carbon Steel
Manufacturer Latrobe Steel
Trade Name Lescalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe Lescalloy® M50 VIM-VAR High Performance Bearing Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LESCALLOY M50 VIM-VAR steel is a through-hardening grade with high hardness and high compressive strength at elevated temperatures. It is produced exclusively as a double vacuum melted produced using vacuum induction melting plus VAC-ARC remelting. This VIM-ARC process provides the optimum in control and reproducibility of chemistry, micro cleanliness and superior fatigue resistance.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Density 8.03 g/cc
0.290 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 62
62
RT
35

@Temperature 649 °C
35

@Temperature 1200 °F
55

@Temperature 482 °C
55

@Temperature 900 °F
60

@Temperature 204 °C
60

@Temperature 400 °F
Modulus of Elasticity 203 GPa
29500 ksi
86.2 GPa

@Temperature 649 °C
12500 ksi

@Temperature 1200 °F
148 GPa

@Temperature 316 °C
21500 ksi

@Temperature 600 °F
Machinability 65 %
65 %
1% Carbon Tool
Thermal Properties Metric English Comments
CTE, linear 10.06 µm/m-°C

@Temperature -73.0 - 21.0 °C
5.589 µin/in-°F

@Temperature -99.4 - 69.8 °F
11.5 µm/m-°C

@Temperature 21.0 - 149 °C
6.39 µin/in-°F

@Temperature 69.8 - 300 °F
13.28 µm/m-°C

@Temperature 21.0 - 538 °C
7.378 µin/in-°F

@Temperature 69.8 - 1000 °F
Component Elements Properties Metric English Comments
Carbon, C 0.85 %
0.85 %
Chromium, Cr 4.1 %
4.1 %
Iron, Fe 89.3 %
89.3 %
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo 4.25 %
4.25 %
Silicon, Si 0.20 %
0.20 %
Vanadium, V 1.0 %
1.0 %