Polymer Property : CTE, linear = 11.56 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 11.56 µm/m-°C

@Temperature 25.0 - 538 °C
6.422 µin/in-°F

@Temperature 77.0 - 1000 °F
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Longitudinal Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..
CTE, linear 11.56 µm/m-°C

@Temperature 25.0 - 538 °C
6.422 µin/in-°F

@Temperature 77.0 - 1000 °F
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Transverse Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..
CTE, linear 11.56 µm/m-°C

@Temperature 25.0 - 538 °C
6.422 µin/in-°F

@Temperature 77.0 - 1000 °F
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Longitudinal Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..
CTE, linear 11.56 µm/m-°C

@Temperature 25.0 - 538 °C
6.422 µin/in-°F

@Temperature 77.0 - 1000 °F
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Transverse Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..