Polymer Property : CTE, linear = 11.26 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 11.26 µm/m-°C

@Temperature 24.0 - 93.0 °C
6.256 µin/in-°F

@Temperature 75.2 - 199 °F
Latrobe Lesco 53 VIM-VAR Premium Carburizing Steel
LESCO 53 VIM-VAR is a premium quality alloy carburizing gear steel designed to resist softening at elevated service temperatures. It is double vacuum processed by vacuum induction melting followed ..
CTE, linear 11.26 µm/m-°C

@Temperature 25.0 - 900 °C
6.256 µin/in-°F

@Temperature 77.0 - 1650 °F
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)
Data provided by Carpenter Technology Corporation.Kovar® alloy is a vacuum melted, Fe-Ni-Co, low expansion alloy whose chemical composition is controlled within narrow limits to assure precise unif..
CTE, linear 11.26 µm/m-°C

@Temperature 24.0 - 93.0 °C
6.256 µin/in-°F

@Temperature 75.2 - 199 °F
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties
Data provided by Carpenter Technology Corporation.This is a carburizing steel possessing good temper resistance and high case hot hardness while maintaining high core impact strength and fracture to..