Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.5 - 18.5 µm/m-°C @Temperature 20.0 - 200 °C |
9.72 - 10.3 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
CTE, linear | 17.5 - 18.5 µm/m-°C @Temperature 20.0 - 200 °C |
9.72 - 10.3 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T7 Heat Treatment Condition T7 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
CTE, linear | 17.5 - 18.5 µm/m-°C @Temperature 20.0 - 200 °C |
9.72 - 10.3 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6 Heat Treatment Condition T6 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |