Polymer Property : Active Range = 300 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Active Range 100 - 300 °C
212 - 572 °F
Indium Corp. Indalloy® 84157 Flux #5-0A Clear Liquid Flux
Indalloy Flux #5-0A is a clear liquid flux formulated for the purpose of soldering moderately easy to difficult metallizations such as nickel, oxidized copper, Kovar and brass. This flux contains o..