Indium Corp. Indalloy® 84157 Flux #5-0A Clear Liquid Flux

Category Fluid
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 84157 Flux #5-0A Clear Liquid Flux.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Indalloy Flux #5-0A is a clear liquid flux formulated for the purpose of soldering moderately easy to difficult metallizations such as nickel, oxidized copper, Kovar and brass. This flux contains organic salts in a water-free water-soluble solvent.Cleaning: Warm water (< 50°C) and detergentSolder Alloy Compatibility: Indalloy Flux #5-0A works well with all types of soft solders.Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Solids Content 30 %
30 %
Thermal Properties Metric English Comments
Active Range 100 - 300 °C
212 - 572 °F
Flash Point 143 °C
289 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified