Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 17.7 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
9.83 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP511ES Glass Epoxy Laminate
Description: NP511ES is a woven glass fabric with high temperature, static dissipative epoxy resin. It has excellent mechanical strength and electrical properties at elevated temperatures with a con..