Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 142 µm/m-°C @Temperature -40.0 - 40.0 °C |
78.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA High flow PPO+PA. Power distribution box applications. |
|||
CTE, linear, Transverse to Flow | 142 µm/m-°C @Temperature -40.0 - 40.0 °C |
78.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific) High flow PPO+PA. Power distribution box applications. |
|||
CTE, linear, Transverse to Flow | 142 µm/m-°C @Temperature 23.0 - 200 °C |
78.9 µin/in-°F @Temperature 73.4 - 392 °F |
ASTM D696 |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
CTE, linear, Transverse to Flow | 142 µm/m-°C @Temperature 23.0 - 200 °C |
78.9 µin/in-°F @Temperature 73.4 - 392 °F |
ASTM D696 |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
CTE, linear, Transverse to Flow | 142 µm/m-°C @Temperature 20.0 °C |
78.9 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® RS 76E101 Nylon 66 Alloy, Rigid Grade (Conditioned) RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properti.. |