Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 50.0 - 136 µm/m-°C | 27.8 - 75.6 µin/in-°F | Average value: 78.2 µm/m-°C Grade Count:22 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
CTE, linear, Transverse to Flow | 67.0 - 136 µm/m-°C | 37.2 - 75.6 µin/in-°F | Average value: 90.0 µm/m-°C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |