Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX1814N PC |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX1832 PC MFR=3.0; Branched extrusion grade for LED applications, UV stabilized; available in diffuse colors |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9610 PC (Asia Pacific) Lexan LUX9610 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS require.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9612G PC (Europe-Africa-Middle East) Lexan LUX9612G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9616 PC (Asia Pacific) Lexan LUX9616 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9616G PC (Asia Pacific) Lexan LUX9616G is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requirem.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
37.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP FARADEX DX92079 PC (Europe-Africa-Middle East) LNP* Faradex* DX92079 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Bead, Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding, Mold Release... |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
37.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP FARADEX NX96302 PC+ABS LNP* FARADEX* NX96302 is a compound based on PC+ABS resin containing Stainless Steel Fibers. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXRL2032 PC (Asia Pacific) Lexan EXRL2032 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS requir.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9616G PC (Europe-Africa-Middle East) Lexan LUX9616G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® PPF-165A Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A conventional molding compound specifically formulated for semiconductor devices which are molded with preplated leadframes. Lo.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C | 37.2 µin/in-°F | ASTM D696 |
Kuraray Genestarâ„¢ N1006A-M41 Nylon Impact modified unreinforced injection grade. Main Features:High elongationHigh impact strengthExamples of applications are:Retainers for quick connectorFlexible band |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
37.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V9561 PET Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DX11355 PC (Asia Pacific) This is a PC based compound with good plating, surface, mechanical performance and flame retardant (Halogen free), a good candidate for Laser Direct Structuring applications. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
37.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXY PA 66 LNP* Thermocomp* RF006XXY is a compound based on Nylon 66 containing 30% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
37.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp RX06027 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RX06027 is a compound based on PA 66 containing Glass Bead. Added features include: Easy Molding, Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-A.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
37.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP WH0200B PBT LNP* Thermocomp* WH0200B is a compound based on PBT resin containing proprietary fillers. Added features include: High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
37.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF RN001IX4 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RN001X4 is a compound based on PA 66 resin containing MoS2. Added features include: Internally Lubricated, High Impact, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
37.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP NF0061 PC+ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* NF0061 is a compound based on PC+ABS resin containing Glass Fiber, Flame Retardant. Added features include : Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
37.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp WB008 PBT LNP* Thermocomp* WB008 is a compound based on Thermoplastic Polyester (PBT) containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makroblend® EL-700 Polycarbonate + Polyester Blend Key Features:Flame retarding agentUnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makroblend® UT-400 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makroblend® UT-403 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
37.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RX06027 PA66, 30% Glass Filled, Injection Molded Staramide RX06027 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S34/8)Information provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® KU 2-1466 Polycarbonate/ABS Blend Flame retardant grade with 20% glass fiber reinforcement, high stiffness.Applications: Electrical industry.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated f.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makroblend® UT-250 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C | 37.2 µin/in-°F | ISO 11359 |
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
37.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
CTE, linear, Transverse to Flow | 67.0 - 136 µm/m-°C | 37.2 - 75.6 µin/in-°F | Average value: 90.0 µm/m-°C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |