Polymer Property : CTE, linear, Transverse to Flow = 67.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 43.0 - 67.0 µm/m-°C

@Temperature 50.0 - 300 °C
23.9 - 37.2 µin/in-°F

@Temperature 122 - 572 °F
Average value: 54.5 µm/m-°C Grade Count:2
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va..