Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 43.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
23.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36EU PC LNP* Lubricomp* DFL36EU is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Easy Molding and UV Stabilized. |
|||
CTE, linear, Transverse to Flow | 43.0 - 67.0 µm/m-°C @Temperature 50.0 - 300 °C |
23.9 - 37.2 µin/in-°F @Temperature 122 - 572 °F |
Average value: 54.5 µm/m-°C Grade Count:2 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
CTE, linear, Transverse to Flow | 43.0 µm/m-°C | 23.9 µin/in-°F | |
Idemitsu Kosan Xarec® N WA 5030 SPS, 30% Glass Filled |
|||
CTE, linear, Transverse to Flow | 43.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
23.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RCL26 PA6.6 LNP* LUBRICOMP* RCL26 is a compound based on Nylon 66 containing 30% Carbon Fiber, 10% PTFE. Added features of this grade include: Wear Resistant, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 43.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON EX11318C PEI (Asia Pacific) LNP* Stat-Kon* EX11318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
CTE, linear, Transverse to Flow | 43.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
23.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 43.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP UF00ASW PPA LNP* Thermocomp* UF00ASW is a compound based on Polyphthalamide (PPA) containing glass fiber. Characteristics of this grade of Heat Stabilized and Hot Water Moldable. |
|||
CTE, linear, Transverse to Flow | 43.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
23.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers. |
|||
CTE, linear, Transverse to Flow | 43.0 µm/m-°C @Temperature 50.0 - 200 °C |
23.9 µin/in-°F @Temperature 122 - 392 °F |
DIN 53 752 |
Ensinger TECASINT 1101 Polyimide (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
CTE, linear, Transverse to Flow | 43.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
23.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP PH0800A PA 6 LNP* THERMOCOMP* PH0800A is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity. |