Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 66.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EX1632T PC
Lexan* EX1632T polycarbonate resin is designed for use in multi-wall sheet or profile extrusion applications. It contains branched polycarbonate resin, release, and UV stabilizer. It is available ..
CTE, linear, Transverse to Flow 66.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
36.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP OL003A PPS - Branched
LNP* LUBRICOMP* OL003A is a compound based on PPS - Branched resin containing 15% PTFE. Added features of this grade are: Wear Resistant.
CTE, linear, Transverse to Flow 66.0 µm/m-°C

@Temperature 0.000 - 200 °C
36.7 µin/in-°F

@Temperature 32.0 - 392 °F
TMA; ASTM E831
Solvay Specialty Polymers Xydar® MG-850 Liquid Crystal Polymer (LCP), 50% GlassMineral
Xydar® MG-850 liquid crystal polymer (LCP) is a 50% glass/mineral reinforced injection molding grade developed for electrical/electronic applications utilizing surface mount technology. The mater..
CTE, linear, Transverse to Flow 66.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
36.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON DX98477 PC
LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
CTE, linear, Transverse to Flow 66.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
36.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon ZEL34XXC PPE+PS (Europe-Africa-Middle East)
LNP* Stat-kon* ZEL34XXC is a compound based on PPE+PS Blend resin containing Carbon Fiber, PTFE. Added features include : Electrically Conductive , Internally Lubricated.This data was supplied by S..
CTE, linear, Transverse to Flow 66.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
36.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS
LNP* THERMOCOMP* AF004L is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Low Extractible.
CTE, linear, Transverse to Flow 66.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
36.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon DE0049 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DC-1004 FR is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.This..
CTE, linear, Transverse to Flow 66.0 µm/m-°C
36.7 µin/in-°F
dry; ISO 11359-1/-2
DSM EcoPaXX® Q-KG6 PA410-GF30
% Glass Reinforced, Heat Stabilized, for E&E applications
CTE, linear, Transverse to Flow 66.0 µm/m-°C
36.7 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Heat Stabilized Polyamide 66 Minlon 10B40HS1 BK061 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe..
CTE, linear, Transverse to Flow 66.0 µm/m-°C
36.7 µin/in-°F
dry; ISO 11359-1/-2
DSM EcoPaXX® Q-HG6 PA410-GF30
30% Glass Reinforced, Heat Stabilized
CTE, linear, Transverse to Flow 66.0 µm/m-°C
36.7 µin/in-°F
dry; ISO 11359-1/-2
DSM EcoPaXX® Q-KGS6 PA410-GF30 FR
30% Glass Reinforced, Flame Retardant (Halogen free)