Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 48.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 48.0 µm/m-°C

@Temperature 20.0 °C
26.7 µin/in-°F

@Temperature 68.0 °F
Eastman Eastapak 7352 PET  (discontinued **)
Unreinforced Low IV. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003.
CTE, linear, Transverse to Flow 48.0 µm/m-°C

@Temperature 20.0 °C
26.7 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1, -2
LNP Thermocomp® LF-1006 Polyetheretherketone, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
CTE, linear, Transverse to Flow 48.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL ZM3640 PPE+PS (Asia Pacific)
CTE, linear, Transverse to Flow 48.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON DE003Z PC
LNP STAT-KON* DE003Z is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Extrusion Grade.
CTE, linear, Transverse to Flow 48.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON RE006 PA 66
LNP STAT-KON* RE006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 48.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp 9X06477 SPS
LNP* Thermocomp* 9X06477 is a compound based on Syndiotactic Polystyrene resin containing Glass Fiber. Characteristics of this grade is Heat Stabilized.This data was supplied by SABIC-IP for the Am..
CTE, linear, Transverse to Flow 48.0 µm/m-°C

@Temperature 20.0 °C
26.7 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Teijin Multilon DN-1520B Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 20 % filler. Improved stiffness and high fluidity realizes a thin wall..
CTE, linear, Transverse to Flow 48.0 µm/m-°C

@Temperature 20.0 °C
26.7 µin/in-°F

@Temperature 68.0 °F
Toyobo TS201 HS PPS, Glass Fiber/Mineral Reinforced
Key Feature: High stiffness, high toughnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excel..
CTE, linear, Transverse to Flow 48.0 µm/m-°C

@Temperature 20.0 °C
26.7 µin/in-°F

@Temperature 68.0 °F
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced
Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel..
CTE, linear, Transverse to Flow 48.0 µm/m-°C
26.7 µin/in-°F
dry; ISO 11359-1/-2
DSM Stanyl® TC154 PA46 FR(17)
Thermal conductive material, Flame Retardant, Heat Stabilized
CTE, linear, Transverse to Flow 48.0 µm/m-°C
26.7 µin/in-°F
z, below Tg; IPC TM-650 2.4.24
Arlon 84N Polyimide Laminate and Prepreg
84N is a high performance ceramic-filled polyimide prepreg based on Arlon's 85N pure polyimide system, designed for use in filling etched areas in polyimide multilayers that contain thick copper lay..
CTE, linear, Transverse to Flow 48.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP VERTON RV0079 PA 66
LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing 35% Long Glasss Fiber. Added features of this material include: Flame Retardant, Structural.
Copyright © lookpolymers.com All Rights Reserved