Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 46.8 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics Lexan® LGK3020 PC (Asia Pacific)
Glass reinforced. Flame retardant.
CTE, linear, Transverse to Flow 46.8 - 113 µm/m-°C
26.0 - 62.8 µin/in-°F
Average value: 86.1 µm/m-°C Grade Count:20
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
CTE, linear, Transverse to Flow 46.8 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC
LNP* Thermocomp* Lexan_LGK3020 compound is a glass reinforced. Flame retardant.
CTE, linear, Transverse to Flow 46.8 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC (Europe-Africa-Middle East)
LNP* Thermocomp* Lexan_LGK3020 compound is a glass reinforced, flame retardant material.
CTE, linear, Transverse to Flow 46.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS
LNP* Thermodcomp* Noryl_PCN2910 compound is a 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market.
CTE, linear, Transverse to Flow 46.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS (Asia Pacific)
35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market.
CTE, linear, Transverse to Flow 46.8 - 46.8 µm/m-°C

@Temperature 100 - 100 °C
26.0 - 26.0 µin/in-°F

@Temperature 212 - 212 °F
Average value: 46.8 µm/m-°C Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is..
CTE, linear, Transverse to Flow 46.8 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC (Asia Pacific)
Glass reinforced. Flame retardant.