Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 33.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.3 µin/in-°F @Temperature -40.0 - 203 °F |
|
PTS Tristar® PC-10R-CL02(V38) 38 MFI Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear, Transverse to Flow | 33.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP COLORCOMP DX98550H PC LNP* COLORCOMP* DX98550H is an unfilled Polycarbonate resin. Added features of this grade are: Low Extractable, Healthcare. |
|||
CTE, linear, Transverse to Flow | 33.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
18.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RFP38 PA6.6 LNP* LUBRICOMP* RFP38 is a compound based on Nylon 66 containing 40% Glass Fiber, 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 33.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 33.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
18.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 33.0 µm/m-°C | 18.3 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America Epiall® 1914A Short Glass Fiber Reinforced Epoxy Epiall 1914A is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided by.. |
|||
CTE, linear, Transverse to Flow | 33.0 µm/m-°C | 18.3 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America RX® 680 Fiberglass and Glass Reinforced Phenolic RX 680 is a fiberglass and glass bead filled phenolic molding compound, with good dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bak North America,.. |