Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 28.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA
LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized.
CTE, linear, Transverse to Flow 28.0 µm/m-°C
15.6 µin/in-°F
TMA
Vyncolit TX10916 Graphite Filled Novolac Phenolic
Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is required.Information provided by Sumitomo Bak North America, Inc.
CTE, linear, Transverse to Flow 28.0 µm/m-°C

@Temperature 20.0 °C
15.6 µin/in-°F

@Temperature 68.0 °F
Goodfellow Carbon/Epoxy Composite Rod
Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow.