Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 50.0 - 150 µm/m-°C
27.8 - 83.3 µin/in-°F
Average value: 110 µm/m-°C Grade Count:3
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
CTE, linear, Transverse to Flow 80.0 - 150 µm/m-°C
44.4 - 83.3 µin/in-°F
Average value: 133 µm/m-°C Grade Count:6
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
CTE, linear, Transverse to Flow 50.0 - 150 µm/m-°C
27.8 - 83.3 µin/in-°F
Average value: 110 µm/m-°C Grade Count:9
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
CTE, linear, Transverse to Flow 80.0 - 150 µm/m-°C
44.4 - 83.3 µin/in-°F
Average value: 97.0 µm/m-°C Grade Count:12
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
CTE, linear, Transverse to Flow 56.0 - 150 µm/m-°C

@Temperature 50.0 - 250 °C
31.1 - 83.3 µin/in-°F

@Temperature 122 - 482 °F
Average value: 104 µm/m-°C Grade Count:5
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..
CTE, linear, Transverse to Flow 150 - 150 µm/m-°C

@Temperature 60.0 - 138 °C
83.3 - 83.3 µin/in-°F

@Temperature 140 - 280 °F
Average value: 150 µm/m-°C Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled