Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 147 µm/m-°C

@Temperature 20.0 °C
81.7 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 180A-28(HT) Cellulose Acetate  (discontinued **)
28% Plasticized.ISO data as provided by the manufacturer, Eastman Chemical.
CTE, linear, Transverse to Flow 147 µm/m-°C

@Temperature -30.0 - 100 °C
81.7 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 9710 PP
SABIC® PPcompound 9710 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st..