Polymer Property : CTE, linear, Transverse to Flow = 13.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 13.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
7.22 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP510A Glass Fabric
Description: Woven glass fabric epoxy laminate. Engineered to provide NEMA grade FR-4 properties. This material contains bromine on the epoxy resin backbone. Certifiable to MIL-I-24768/27, Type GEE-..
CTE, linear, Transverse to Flow 13.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
7.22 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP634 Laminate
Description: Warm punching, composite grade with woven glass covers for improved flexural, tensile and impact strength. Electrical properties comparable to NP611.Thickness Tested: 0.062", 0.125" and..
CTE, linear, Transverse to Flow 13.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
7.22 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP660 Paper Base Laminate
Description: Lower cost paper phenolic NEMA Grade XP. Uses natural kraft paper without pigmented cover sheet. Warm to hot punching. UL listed. Thickness Tested: 0.062", 0.125" & 0.500"
CTE, linear, Transverse to Flow 13.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
7.22 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis
Industrial Laminates/Norplex P95 Glass Fabric
Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested..
CTE, linear, Transverse to Flow 13.0 µm/m-°C

@Temperature 23.0 °C
7.22 µin/in-°F

@Temperature 73.4 °F
Alliance S-20A Samarium Cobalt Magnetic Material
CTE, linear, Transverse to Flow 13.0 µm/m-°C

@Temperature 23.0 °C
7.22 µin/in-°F

@Temperature 73.4 °F
Alliance S-20B Samarium Cobalt Magnetic Material
CTE, linear, Transverse to Flow 13.0 µm/m-°C

@Temperature 23.0 °C
7.22 µin/in-°F

@Temperature 73.4 °F
Alliance S-26A Samarium Cobalt Magnetic Material
CTE, linear, Transverse to Flow 13.0 µm/m-°C

@Temperature 23.0 °C
7.22 µin/in-°F

@Temperature 73.4 °F
Alliance S-22A Samarium Cobalt Magnetic Material
CTE, linear, Transverse to Flow 13.0 µm/m-°C

@Temperature 23.0 °C
7.22 µin/in-°F

@Temperature 73.4 °F
Alliance S-22B Samarium Cobalt Magnetic Material