Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 23.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI (Asia Pacific)
LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive.