Polymer Property : CTE, linear, Transverse to Flow = 109 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 109 µm/m-°C

@Temperature 23.0 - 60.0 °C
60.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON RX06001 PA 66 (Europe-Africa-Middle East)
LNP* Stat-kon* RX06001 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Easy Molding, High Impact, Electrically Conductive.
CTE, linear, Transverse to Flow 109 µm/m-°C

@Temperature -30.0 - 30.0 °C
60.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-LOY A3000TXB ABS
LNP* STAT-LOY* A3000TXB is a compound based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives and Bioassessed to ISO 10993...
CTE, linear, Transverse to Flow 109 µm/m-°C

@Temperature -30.0 - 30.0 °C
60.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP HX03408 PA11
LNP* Thermocomp* HX03408 is a compound based on Nylon 11 containing Proprietary Fillers. Added feature includes: Clean Compound System
CTE, linear, Transverse to Flow 109 µm/m-°C

@Temperature -30.0 - 30.0 °C
60.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP TH0300B PU
LNP* Thermocomp* Th0300B is a compound based on Polyurethane containing proprietary fillers. Characteristics of this grade are High Specific Gravity.
CTE, linear, Transverse to Flow 109 µm/m-°C

@Temperature -30.0 - 30.0 °C
60.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP
LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.
CTE, linear, Transverse to Flow 109 µm/m-°C

@Temperature 23.0 - 60.0 °C
60.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam RF0052E PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam RF0052E is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding ResinInformation provided by Eurostar.