Polymer Property : Heat Distortion Temperature = 167 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature 75.0 °C

@Pressure 0.450 MPa
167 °F

@Pressure 65.3 psi
ISO 75A-1
Iran Petrochemical (PCC) HB5020 High Density Polyethylene
HB-5020 is a high molecular weight high density polyethylene.Applications: extrusion blow moldingInformation provided by Iran Petrochemical Commercial Co.