Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) HB5020 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) HB5020 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HB-5020 is a high molecular weight high density polyethylene.Applications: extrusion blow moldingInformation provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Melt Flow 0.22 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.22 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
1.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
20 g/10 min

@Load 21.6 kg,
Temperature 190 °C
20 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527-1
Elongation at Yield 9.0 %
9.0 %
ISO 527-1
Tensile Modulus 1.00 GPa
145 ksi
ISO 527-1
Tensile Impact Strength 100 kJ/m²

@Temperature -30.0 °C
47.6 ft-lb/in²

@Temperature -22.0 °F
ISO 8256
Thermal Properties Metric English Comments
Vicat Softening Point 78.0 °C
172 °F
ISO 306
Heat Distortion Temperature 43.0 °C

@Pressure 1.80 MPa
109 °F

@Pressure 261 psi
ISO 57B-1
75.0 °C

@Pressure 0.450 MPa
167 °F

@Pressure 65.3 psi
ISO 75A-1
Processing Properties Metric English Comments
Melt Temperature 131 °C
268 °F
Users viewing this material also viewed the following: