Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 43.0 °C @Pressure 1.80 MPa |
109 °F @Pressure 261 psi |
ISO 57B-1 |
Iran Petrochemical (PCC) HB5020 High Density Polyethylene HB-5020 is a high molecular weight high density polyethylene.Applications: extrusion blow moldingInformation provided by Iran Petrochemical Commercial Co. |