Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C @Thickness 3.18 mm |
174 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L6607 Polyvinyl Chloride, Rigid (PVC, Rigid) Physical properties based on Geon L6607 white 1363Information provided by PolyOne |