Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C @Thickness 3.18 mm |
174 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L6607 Polyvinyl Chloride, Rigid (PVC, Rigid) Physical properties based on Geon L6607 white 1363Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 6.40 mm |
174 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 6.40 mm |
174 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications. |