Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 76.2 °C @Treatment Temp. 60.0 °C, Thickness 3.18 mm |
169 °F @Treatment Temp. 140 °F, Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO.. |