Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 304 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 151 °C

@Thickness 3.20 mm
304 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL PKN4752 PPE+PS
PPE+PS blend. High Heat. Translucent with yellow tint in natural color. FDA compliant. Extrusion and Injection Molding. Typical applications include High Performance Food Packaging, Electronics and ..
Deflection Temperature at 1.8 MPa (264 psi) 151 °C

@Thickness 6.40 mm
304 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL PKN4752 PPE+PS
PPE+PS blend. High Heat. Translucent with yellow tint in natural color. FDA compliant. Extrusion and Injection Molding. Typical applications include High Performance Food Packaging, Electronics and ..
Deflection Temperature at 1.8 MPa (264 psi) 151 °C

@Thickness 3.20 mm
304 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Asia Pacific)
PPE+PS. Translucent. FDA compliant. High heat. Extrusion. Microwavable. Food, electrical/electronic packaging uses.
Deflection Temperature at 1.8 MPa (264 psi) 151 °C

@Thickness 6.40 mm
304 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Asia Pacific)
PPE+PS. Translucent. FDA compliant. High heat. Extrusion. Microwavable. Food, electrical/electronic packaging uses.