Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C @Thickness 3.20 mm |
304 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS PPE+PS blend. High Heat. Translucent with yellow tint in natural color. FDA compliant. Extrusion and Injection Molding. Typical applications include High Performance Food Packaging, Electronics and .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C @Thickness 6.40 mm |
304 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS PPE+PS blend. High Heat. Translucent with yellow tint in natural color. FDA compliant. Extrusion and Injection Molding. Typical applications include High Performance Food Packaging, Electronics and .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C @Thickness 3.20 mm |
304 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High heat. Extrusion. Microwavable. Food, electrical/electronic packaging uses. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C @Thickness 6.40 mm |
304 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High heat. Extrusion. Microwavable. Food, electrical/electronic packaging uses. |