Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 143 °C

@Thickness 4.00 mm
289 °F

@Thickness 0.157 in
Annealed; ASTM D648
LG Chemical Lupoy 1200-03 Polycarbonate Resin
Description: LUPOY PC 1200-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 143 °C

@Thickness 4.00 mm
289 °F

@Thickness 0.157 in
Annealed; ASTM D648
LG Chemical Lupoy 1201-05 Polycarbonate Resin
Description: LUPOY PC 1201-05 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 143 °C

@Thickness 4.00 mm
289 °F

@Thickness 0.157 in
Annealed; ASTM D648
LG Chemical Lupoy 1261-03 Polycarbonate Resin
Description: LUPOY PC 1261-03 resin is designed for extrusion blow molding(EBM) and injection stretch blow molding (ISBM) products. It exhibits an excellent physical property balance of heat resista..
Deflection Temperature at 1.8 MPa (264 psi) 143 °C

@Thickness 4.00 mm
289 °F

@Thickness 0.157 in
Annealed; ASTM D648
LG Chemical Lupoy 1302-05 Polycarbonate Resin
Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main..
Deflection Temperature at 1.8 MPa (264 psi) 143 °C

@Thickness 4.00 mm
289 °F

@Thickness 0.157 in
Annealed; ASTM D648
LG Chemical Lupoy 1600-03 Polycarbonate Resin
Description: LUPOY PC 1600-03 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics: ..
Deflection Temperature at 1.8 MPa (264 psi) 143 °C

@Thickness 4.00 mm
289 °F

@Thickness 0.157 in
Annealed; ASTM D648
LG Chemical Lupoy 1603-03 Polycarbonate Resin
Description: LUPOY PC 1603-03 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics: ..
Deflection Temperature at 1.8 MPa (264 psi) 143 °C

@Thickness 4.00 mm
289 °F

@Thickness 0.157 in
Annealed; ASTM D648
LG Chemical Lupoy 1300-03 Polycarbonate Resin
Description: LUPOY PC 1300-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...