Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 150 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 65.6 °C

@Thickness 10.0 - 25.0 mm
150 °F

@Thickness 0.394 - 0.984 in
ASTM D648
CPC - Vycom CELTEC® Expanded Rigid foam PVC board
Celtec Displayboard is a foamed polyvinyl chloride (PVC) sheet whose combination of features makes it ideal for signage, exhibits, store displays, POP, Kiosks, screen printing and more. The surface..