Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 103 °C

@Thickness 6.40 mm
217 °F

@Thickness 0.252 in
unannealed; ASTM D 648
SABIC Innovative Plastics Cycolac® GHT3330 ABS (Asia Pacific)
High heat grade of ABS used for interior automotive components.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 1.8 MPa (264 psi) 103 °C

@Thickness 6.40 mm
217 °F

@Thickness 0.252 in
unannealed; ASTM D 648
SABIC Innovative Plastics Cycolac® Z48 ABS
Automotive. Very high heat resistance with medium impact and good strength properties.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 1.8 MPa (264 psi) 103 °C

@Thickness 6.40 mm
217 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics PREVEX W20 PPE+PS (Asia Pacific)
Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F.
Deflection Temperature at 1.8 MPa (264 psi) 103 °C

@Thickness 6.40 mm
217 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics PREVEX W20 PPE+PS
Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F.