SABIC Innovative Plastics PREVEX W20 PPE+PS

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Prevex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics PREVEX W20 PPE+PS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0060 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D785
Tensile Strength, Yield 40.0 MPa
5800 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 52 %
52 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 1.93 GPa
280 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 62.0 MPa
8990 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2.03 GPa
294 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D256
2.13 J/cm

@Temperature -30.0 °C
3.99 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Gardner Impact 37.0 J
27.3 ft-lb
ASTM D3029
27.0 J

@Temperature -40.0 °C
19.9 ft-lb

@Temperature -40.0 °F
ASTM D3029
29.0 J

@Temperature -30.0 °C
21.4 ft-lb

@Temperature -22.0 °F
ASTM D3029
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 79.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C

@Thickness 3.20 mm
208 °F

@Thickness 0.126 in
unannealed; ASTM D648
103 °C

@Thickness 6.40 mm
217 °F

@Thickness 0.252 in
unannealed; ASTM D648