Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 67.2 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 67.2 °C

@Thickness 3.18 mm
153 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid)
Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: ..
Deflection Temperature at 0.46 MPa (66 psi) 67.2 °C

@Thickness 3.18 mm
153 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ SF M7000 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 67.2 °C

@Thickness 3.18 mm
153 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ SF M7010 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 67.2 °C

@Thickness 3.18 mm
153 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ SF M7020 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne