Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 67.2 °C @Thickness 3.18 mm |
153 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid) Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 67.2 °C @Thickness 3.18 mm |
153 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ SF M7000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 67.2 °C @Thickness 3.18 mm |
153 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ SF M7010 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 67.2 °C @Thickness 3.18 mm |
153 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ SF M7020 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |