Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 148 °C @Thickness 3.20 mm |
298 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000 PC (Asia Pacific) |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 148 °C @Thickness 6.40 mm |
298 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000 PC (Asia Pacific) |