Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 266 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C

@Thickness 6.40 mm
266 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific)
NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C