Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C

@Thickness 3.20 mm
212 °F

@Thickness 0.126 in
Annealed; ASTM-D648
Ineos ABS Lustran® 308 ABS, Medical Grade
Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi..
Deflection Temperature at 0.46 MPa (66 psi) 100 °C

@Thickness 12.7 mm
212 °F

@Thickness 0.500 in
Annealed; ASTM-D648
Ineos ABS Lustran® ABS 248FC Medical & Food Contact Grade
Lustran® ABS 248FC resin is a high-gloss, medium-impact grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of physical properties and has been desi..