Material Notes:
Lustran® ABS 248FC resin is a high-gloss, medium-impact grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of physical properties and has been designed to be compliant with both medical and food contact regulations. Lustran® ABS 248FC resin is used in applications requiring rigidity and intermediate abuse resistance. As with any product, use of Lustran® ABS 248FC resin in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability. Lustran® ABS 248FC 000000 (natural) complies with FDA regulation 21 CFR 181.32 for repeated-use food-contact applications. It is also compliant with EU Directive 2002/72/EC and its amendments (2004/1/EC, 2004/19/EC, 2005/79/EC, 2008/39/EC) relating to plastic materials and articles intended to come into contact with foodstuffs. Lustran® ABS 248FC resin is designated as “medical-grade” and has met the requirements of the USP Class VI and ISO 10993, Part I “Biological Evaluation of Medical Devices” tests with human tissue contact time of 30 days or less. Regrind must not be used in medical applications requiring biocompatibility. Lustran® ABS 248FC can be made available (upon request) in colors that are compliant with both biocompatibility and food contact requirements.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM-D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM-D955
Melt Flow 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM-D785
Tensile Strength, Yield 47.0 MPa
6820 psi
ASTM-D638
Tensile Modulus 2.60 GPa
377 ksi
ASTM-D638
Flexural Yield Strength 74.0 MPa
10700 psi
ASTM-D790
Flexural Modulus 2.70 GPa
392 ksi
ASTM-D790
Izod Impact, Notched 0.480 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
0.899 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM-D256
2.24 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.20 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
CTE, linear 81.0 µm/m-°C
45.0 µin/in-°F
ASTM-D696
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C

@Thickness 12.7 mm
199 °F

@Thickness 0.500 in
Unannealed; ASTM-D648
100 °C

@Thickness 12.7 mm
212 °F

@Thickness 0.500 in
Annealed; ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C

@Thickness 12.7 mm
187 °F

@Thickness 0.500 in
Unannealed; ASTM-D648
96.0 °C

@Thickness 12.7 mm
205 °F

@Thickness 0.500 in
Annealed; ASTM-D648
102 °C

@Thickness 12.7 mm
216 °F

@Thickness 0.500 in
Annealed, Compression Molded; ASTM-D648
Vicat Softening Point 80.0 °C
176 °F
Rate B; ASTM-D1525
Processing Properties Metric English Comments
Rear Barrel Temperature 235 - 250 °C
455 - 482 °F
Injection Molding
Middle Barrel Temperature 240 - 255 °C
464 - 491 °F
Injection Molding
Front Barrel Temperature 245 - 260 °C
473 - 500 °F
Injection Molding
Nozzle Temperature 245 - 260 °C
473 - 500 °F
Injection Molding
Melt Temperature 245 - 265 °C
473 - 509 °F
Injection Molding
Mold Temperature 45.0 - 65.0 °C
113 - 149 °F
Injection Molding
Drying Temperature 71.0 - 77.0 °C

@Time 14400 sec
160 - 171 °F

@Time 4.00 hour
82.0 - 88.0 °C

@Time 7200 sec
180 - 190 °F

@Time 2.00 hour
Moisture Content <= 0.10 %
<= 0.10 %
Dew Point <= -29.0 °C
<= -20.2 °F
inlet air
Injection Pressure 68.9 - 110 MPa
10000 - 16000 psi
Injection Molding
Back Pressure 0.000 - 0.172 MPa
0.000 - 25.0 psi
Injection Molding
Clamp Pressure 30.8 - 61.6 MPa
4470 - 8930 psi
Injection Molding
Cushion <= 0.635 cm
<= 0.250 in
Injection Molding
Descriptive Properties Value Comments
Hold Pressure 50-75% of Injection Pressure, Injection Molding
Injection Speed High
Injection Molding
Screw Compression Ratio 2.5:1
Injection Molding
Screw Length-to-Diameter Ratio >= 20:1
Injection Molding
Screw Speed Moderate, Injection Molding
Shot Weight-to-Machine Capacity Ratio 0.5-0.75
Injection Molding