Polymer Property : Glass Transition Temp, Tg = 86.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 86.0 °C
187 °F
TM R050-25
Resinlab® EP1330LV Heat Cure Epoxy Polymer System
Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application..
Glass Transition Temp, Tg 86.0 °C
187 °F
Plain Cast Resin; ASTM D3418
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Glass Transition Temp, Tg 86.0 °C
187 °F
wet, 121°C cure
Henkel Hysol EA 9695 Film Adhesive
Second generation, low flow, composite bonding film; excellent environmental resistance. Composite structure repair, cure and co-cure with composite laminates. Qualified to Airbus. Data from .050 ps..
Glass Transition Temp, Tg 86.0 °C
187 °F
Plain Cast Resin; ASTM D3418
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Glass Transition Temp, Tg 86.0 °C
187 °F
ETM 300-90
ExxonMobil ESCOREZ™ 5340 Petroleum Hydrocarbon Resin
The Escorez 5300 series resins are water white cycloaliphatic hydrocarbon resins. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, APP an d A..
Glass Transition Temp, Tg 86.0 °C
187 °F
Armstrong A-4/A Epoxy Adhesive
Is a heavy, non-metallic filled, gray paste epoxy that provides excellent thixotropic non-sag bond lines. It can be used for small volume casting applications.Information provided by Ellsworth Adhe..