Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 86.0 °C | 187 °F | TM R050-25 |
Resinlab® EP1330LV Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Glass Transition Temp, Tg | 86.0 °C | 187 °F | Plain Cast Resin; ASTM D3418 |
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Glass Transition Temp, Tg | 86.0 °C | 187 °F | wet, 121°C cure |
Henkel Hysol EA 9695 Film Adhesive Second generation, low flow, composite bonding film; excellent environmental resistance. Composite structure repair, cure and co-cure with composite laminates. Qualified to Airbus. Data from .050 ps.. |
|||
Glass Transition Temp, Tg | 86.0 °C | 187 °F | Plain Cast Resin; ASTM D3418 |
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Glass Transition Temp, Tg | 86.0 °C | 187 °F | ETM 300-90 |
ExxonMobil ESCOREZ™ 5340 Petroleum Hydrocarbon Resin The Escorez 5300 series resins are water white cycloaliphatic hydrocarbon resins. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, APP an d A.. |
|||
Glass Transition Temp, Tg | 86.0 °C | 187 °F | |
Armstrong A-4/A Epoxy Adhesive Is a heavy, non-metallic filled, gray paste epoxy that provides excellent thixotropic non-sag bond lines. It can be used for small volume casting applications.Information provided by Ellsworth Adhe.. |