Polymer Property : Glass Transition Temp, Tg = 646 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 341 °C
646 °F
DSC; ASTM E1356-03
NeXolve Novastrat® 800 Polyimide
High temperature polyimide film with low coefficient of thermal expansion.NeXolve Novastrat® 800 is a high temperature polyimide film with low coefficient of thermal expansion (CTE), ~4 ppm/°C fro..
Glass Transition Temp, Tg 341 °C
646 °F
wet; ASTM D4065
Quantum Composites HTC-9590 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite
HTC-9590 (127-51-3) is a 12K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristic..
Glass Transition Temp, Tg 341 °C
646 °F
wet; ASTM D4065
Quantum Composites HTC-9593 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite
HTC-9593 (127-51-5) is a 3K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristics..