Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 59.3 °C | 139 °F | ASTM E1545-00 |
DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, UV Postcure DescriptionDSM Somos® 12110 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12110 have a cherry-red appearance which tur.. |